Choose the masterbatch type: see the typical let-down ratio and suggested starting point for colour, white, black, antistatic, UV, slip, antiblock, filler and others; then calculate consumption from extruder output.
What is this calculation used for?
Shows how much of which masterbatch type to add and, from that, works out the dosing unit setting and the hourly, per-shift and monthly requirement. Use it to choose a starting ratio when switching to a new colour or additive, and for resin ordering and stock planning.
Loading calculator… (JavaScript required)
Masterbatch types and typical let-down ratios
How much of which masterbatch? The table below shows the typical ratio range by type, what determines the ratio and the most common mistake on the shop floor. When you choose the type in the calculator, the suggested starting ratio is filled in automatically.
| Masterbatch type | Typical ratio | Start | What determines the ratio | Watch out |
|---|---|---|---|---|
| Colour masterbatch | 1–5 % | 2 % | Wall thickness (thin walls and film need a higher ratio), the opacity required, the depth of shade and the natural colour of the base resin. | Below about 1 %, dosing fluctuation shows up as colour variation and streaks; if necessary ask for a more dilute masterbatch. Check that the carrier is compatible with your resin. |
| White masterbatch (titanium dioxide) | 2–8 % | 4 % | The titanium dioxide content of the masterbatch (mostly 50–75 %), the opacity required and the thickness; thin film needs a higher ratio for the same opacity. | For outdoor products ask for a weather-resistant (surface-treated rutile) grade; cheap whites often contain calcium carbonate and have low opacity. |
| Black masterbatch (carbon black) | 1–6 % | 2 % | The carbon black content of the masterbatch (mostly 30–50 %) and the purpose: colour only, or UV protection. | For UV protection (pipe, outdoor use) about 2–2.5 % carbon black in the product is targeted: with a 40 % carbon black masterbatch that means a let-down of about 5–6 %. The 1–2 % used for colour does not give UV protection. |
| Antistatic (migrating type) | 1–4 % | 2 % | Active content, the polymer (migration is slower in PP than in PE), part or film thickness and the relative humidity where the product is used. | The effect builds up as the additive migrates to the surface: measure surface resistivity after a few days of conditioning, not on a freshly molded part. The effect weakens at low humidity. Too much leaves a greasy surface and impairs printing, bonding and welding. |
| UV stabiliser (HALS, UV absorber) | 1–5 % | 2 % | The outdoor service life required, local solar radiation, thickness (thin film needs a higher ratio) and the pigment used. | In greenhouse film, pesticides containing sulphur and chlorine can deactivate HALS-type stabilisers; ask for a pesticide-resistant type. Verify the service-life claim against the manufacturer’s accelerated weathering data. |
| Antioxidant / heat stabiliser | 0.5–2 % | 1 % | The regrind ratio, the residence time of the material in the barrel and the processing temperature. | Yellowing and a rise in melt flow (higher MFI) are signs of degradation. An antioxidant slows degradation, it does not reverse it; reduce residence time and temperature first. |
| Slip agent (erucamide, oleamide) | 0.5–2 % | 1 % | The target coefficient of friction, thickness (in thin film less additive reaches the surface) and the antiblock used alongside. | The effect settles over a few days through migration; do not measure friction straight away. Too much impairs print and lamination adhesion and heat sealing. It is also used in closures to lower the opening torque. |
| Antiblock (silica, talc) | 1–4 % | 2 % | Film thickness, the film’s tendency to block (high in LLDPE and metallocene grades) and the haze that can be accepted. | The higher the ratio, the hazier the film. Antiblock ties up part of the processing aid (PPA); if you use both, adjust the PPA ratio accordingly. |
| Processing aid (PPA, fluoropolymer) | 0.5–2 % | 1 % | The severity of melt fracture (sharkskin), the share of LLDPE and metallocene grades, the die gap and the output rate. | To coat the die surface, the line is first conditioned at a high ratio; once the surface clears, the ratio is reduced. Antiblock and some pigments reduce its effect. |
| Antifog | 1–4 % | 2 % | Film thickness, the application (greenhouse film or food packaging) and how long the effect has to last. | It is a migrating additive; it washes off over time and the effect fades. For food packaging ask for the food-contact compliance document. |
| Filler (calcium carbonate, talc) | 5–30 % | 10 % | The cost target and the loss of mechanical properties that can be accepted; low ratios are used in film and raffia, higher ones in injection molding and sheet. | Density rises: the part gets heavier and part of the saving per kilo is lost, so calculate the cost per part. Impact strength and elongation at break drop, and dimensions change because shrinkage is lower. Dry it if it has picked up moisture. |
| Desiccant (calcium oxide) | 1–5 % | 2 % | The moisture level of the raw material, especially recycled PE and PP. | If the bag is left open it absorbs moisture from the air and loses its effect; keep it sealed. It causes haze and specks in transparent products. It does not replace drying for hygroscopic engineering plastics such as PA, PET and PC. |
| Nucleating agent / clarifier (PP) | 1–3 % | 2 % | The type and content of the active substance and the goal: shorter cycle, higher stiffness or clarity. | Clarifiers only dissolve and work above the minimum melt temperature given by the manufacturer. Because crystallisation speeds up the cycle gets shorter, but shrinkage changes; check the dimensions again. |
| Chemical blowing agent | 0.5–3 % | 1 % | The purpose (a low ratio to remove sink marks, a high one to reduce weight) and the wall thickness. | The decomposition temperature of the blowing agent must match your barrel temperature. In injection molding use a shut-off nozzle and reduce holding pressure and time. It can leave silver streaks on the surface; trial it first on visible surfaces. |
| Flame retardant | 3–25 % | per data sheet | The flammability class required (UL 94 V-2 or V-0), the wall thickness and the polymer; V-0 takes several times the ratio needed for V-2. | No starting ratio is suggested for this type: the class is only valid for a test at a specific wall thickness. Take the ratio from the manufacturer’s technical data sheet and have it tested at your own part thickness; pigments and fillers can change the result. |
How do I find the right masterbatch ratio?
- The ranges here apply to products of common concentration. The ratio in the technical data sheet of your own product always takes precedence; within the same type, active content varies from one manufacturer to another.
- Carrier compatibility: a PE-carrier masterbatch works without problems in PE and PP. In engineering plastics such as ABS, PC, PA, PET and POM use a product with the same polymer as carrier or one approved for that polymer; otherwise delamination at the surface and a loss of mechanical properties occur.
- If you use regrind, account for the masterbatch already in it: regrind is already coloured and contains additives, so add masterbatch only for the virgin material.
- Set the dosing unit to the grams-per-shot value and verify it by weighing; with volumetric units the amount delivered changes when the pellet size changes.
How is it calculated?
- Masterbatch = output (kg/h) × efficiency × dosing ratio
- Masterbatch for 25 kg of resin = 25 × ratio ÷ (100 − ratio)
Other calculators
Clamping force calculation
Required clamping force and machine size from projected area and cavity pressure.
Mold opening stroke calculation
Minimum opening stroke required from part height, runner and robot clearance, distinguishing toggle and direct hydraulic (two-platen) machines.
Shot weight calculation
Part and shot weight from raw material density, and machine capacity utilization.