Polyamide 6 and 66 (nylon)

PA6 + GF15

High strength and wear resistance; becomes very stiff with glass fiber. Absorbs moisture, and its properties change with moisture.

Processing temperatures

Melt (injection) temperature270 °C
Mold surface temperature80 °C
Ejection temperature140 °C

Typical values. They vary (±) with grade and manufacturer; see the data sheet.

Physical properties (typical)

Density1.24 g/cm³
Shrinkage (flow / cross)0.5 / 1.1 %
Specific heat1.45 kJ/kg·K
Thermal conductivity0.28 W/m·K
Latent heat of crystallization (approx.)68 kJ/kg

Drying

Drying is essential (about 80 °C, 4–6 hours; dry air).

For exact conditions see the material data sheet. Drying guide →

Points to watch

  • Moisture affects filling and strength (splay)
  • Dimensions change as the part reaches moisture equilibrium (swelling)
  • Warpage and surface quality in fiber-filled grades

Typical use: Gears, bearings, engine-bay parts, fasteners

Defects common with this material

Other grades in the same family